This test was carried out to verify complete penetration of TSP 99 in the test rings. The procedure involved making the outer surface of test rings to reduce OD from 25 mm to ----mm. Next the rings were further etched in concentrated Nitric acid and OD was finally down to ------mm. These machined and treated rings were then tested again for leakage and all rings passed the test.
Test data